Mechanical Properties Metric English Comments
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC
Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D4812
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6
LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66
LNP* LUBRICOMP* RX05496 is a compound based on Nylon 66 resin containing 30% Mixed Glass, 15% PTFE, Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 (Asia Pacific)
LNP* Lubricomp* RX05496 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Izod Impact, Unnotched 9.01 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DF005 PC
LNP* Thermocomp* DF005 is a compound based on Polycarbonate containing 25% Glass Fiber.
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D256A
Total PPH 3462 Polypropylene, Extrusion Grade
Homopolymer extrusion grade for slit film and fibrillated tapesProcess Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.FDA - FINA 3462 complies with..
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ISO 180
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM  (discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..