SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RX05496 is a compound based on Nylon 66 resin containing 30% Mixed Glass, 15% PTFE, Silicone. Added features of this material include: Wear Resistant.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Tensile Modulus 8.35 GPa
1210 ksi
50 mm/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 6.84 GPa
992 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C

@Thickness 3.20 mm
469 °F

@Thickness 0.126 in
unannealed; ASTM D648