Mechanical Properties Metric English Comments
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6
LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66
LNP* LUBRICOMP* RX05496 is a compound based on Nylon 66 resin containing 30% Mixed Glass, 15% PTFE, Silicone. Added features of this material include: Wear Resistant.
Izod Impact, Unnotched 9.04 J/cm
16.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 (Asia Pacific)
LNP* Lubricomp* RX05496 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated.