Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 9.55 J/cm
17.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
Izod Impact, Unnotched 9.55 J/cm
17.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched 9.55 J/cm
17.9 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 (Asia Pacific)
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched 9.55 J/cm
17.9 ft-lb/in
ASTM D256A
Total PPH 3622 Polypropylene, Injection Molding Grade
General purpose injection molding and extrusion homopolymerGood Processability -- FINA 3622 is engineered for good processability in thin wall multi- cavity molds.Good Clarity -- FINA 3622 has good ..