Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.55 J/cm | 17.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |
|||
Izod Impact, Unnotched | 9.55 J/cm | 17.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched | 9.55 J/cm | 17.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 (Asia Pacific) LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched | 9.55 J/cm | 17.9 ft-lb/in | ASTM D256A |
Total PPH 3622 Polypropylene, Injection Molding Grade General purpose injection molding and extrusion homopolymerGood Processability -- FINA 3622 is engineered for good processability in thin wall multi- cavity molds.Good Clarity -- FINA 3622 has good .. |