Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Tensile Modulus 8.17 GPa
1180 ksi
50 mm/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 7.86 GPa
1140 ksi
ASTM D790
Izod Impact, Notched 1.54 J/cm
2.89 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.55 J/cm
17.9 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C

@Thickness 3.20 mm
428 °F

@Thickness 0.126 in
unannealed; ASTM D648