Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.92 J/cm @Temperature 23.0 °C |
18.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 9.92 J/cm @Temperature 23.0 °C |
18.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC (Asia Pacific) LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 9.95 J/cm | 18.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12 LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact. |