Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.92 J/cm @Temperature 23.0 °C |
18.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 9.92 J/cm @Temperature 23.0 °C |
18.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC (Asia Pacific) LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |