Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Izod Impact, Unnotched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Izod Impact, Unnotched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
North Wood Plastics 60 PP + UNIFILL (40% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Izod Impact, Unnotched | 2.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D4812 |
PolyOne Geon™ 81510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.10 J/cm @Thickness 3.18 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Izod Impact, Unnotched | 2.10 J/cm @Thickness 3.18 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Izod Impact, Unnotched | 2.10 J/cm @Thickness 3.18 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Izod Impact, Unnotched | 2.10 J/cm @Thickness 3.18 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Izod Impact, Unnotched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Adell RQ-18 Copolymer Polypropylene, 40% Mica Reinforced Data provided by Adell Plastics, Inc. |