Polymer Property : Izod Impact, Unnotched = 3.93 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
North Wood Plastics 60 PP + UNIFILL (40% Wood Fiber)
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It..
Izod Impact, Unnotched 2.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D4812
PolyOne Geon™ 81510 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Unnotched 2.10 J/cm

@Thickness 3.18 mm
3.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
Izod Impact, Unnotched 2.10 J/cm

@Thickness 3.18 mm
3.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
Izod Impact, Unnotched 2.10 J/cm

@Thickness 3.18 mm
3.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Izod Impact, Unnotched 2.10 J/cm

@Thickness 3.18 mm
3.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Adell RQ-18 Copolymer Polypropylene, 40% Mica Reinforced
Data provided by Adell Plastics, Inc.