Polymer Property : Izod Impact, Unnotched = 20.3 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 20.3 - 5340 J/cm
38.0 - 10000 ft-lb/in
Average value: 21.0 J/cm Grade Count:16
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..