Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 5.62 ft-lb/in - NB Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.00 J/cm - NB
5.62 ft-lb/in - NB
Average value: 9.28 J/cm Grade Count:70
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler  (discontinued **)
Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa..
Izod Impact, Unnotched 3.00 J/cm
5.62 ft-lb/in
J/cm²; ISO 180A
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide Compound  (Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-220BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications requiring ..
Izod Impact, Unnotched 3.00 - 4.00 J/cm

@Temperature 23.0 °C
5.62 - 7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Loxim 500 00V0 Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Izod Impact, Unnotched 3.00 J/cm
5.62 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Izod Impact, Unnotched 3.00 J/cm

@Temperature -30.0 °C
5.62 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
Izod Impact, Unnotched 3.00 J/cm

@Thickness 3.20 mm
5.62 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 265 Toughened Polystyrene
CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther..