Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.01 J/cm | 11.3 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D4812 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
Izod Impact, Unnotched | 6.01 J/cm | 11.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched | 6.01 J/cm | 11.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX09303C PC (Asia Pacific) LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of thi.. |
|||
Izod Impact, Unnotched | 6.01 J/cm | 11.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber. |