Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.60 - 3.74 J/cm
3.00 - 7.00 ft-lb/in
Average value: 2.67 J/cm Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Izod Impact, Unnotched 1.07 - 3.74 J/cm
2.00 - 7.00 ft-lb/in
Average value: 2.14 J/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..
Izod Impact, Unnotched 3.20 - 3.74 J/cm
6.00 - 7.00 ft-lb/in
Average value: 3.60 J/cm Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..