Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.60 J/cm | 8.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
  AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Izod Impact, Unnotched | 4.60 J/cm | 8.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA), 30% Glass Fiber Ixef® 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance.Features: .. |
|||
Izod Impact, Unnotched | 4.60 - 11.0 J/cm | 8.62 - 20.6 ft-lb/in | Average value: 7.98 J/cm Grade Count:10 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |