Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded  

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded  .pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good dimensional stability; therefore, typical humid environmental conditions result in only minor changes in the strength and stiffness. This grade of AMODEL resin can withstand the demanding vapor phase and infrared reflow soldering processes typically used in the electronics industry. It is ideally suited for most connectors and electrical devices requiring surface mount technology (SMT). The material offers easy processing using conventional equipment and methods.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.MatWeb has an entry for this material conditioned at 50% RH.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Water Absorption 0.18 %
0.18 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM E831
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ASTM E831
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength, Ultimate 179 MPa
26000 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Tensile Modulus 13.8 GPa
2000 ksi
ASTM D638
Flexural Yield Strength 257 MPa
37300 psi
ASTM D790
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.60 J/cm
8.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.00e+15 ohm-cm
3.00e+15 ohm-cm
ASTM D257
Surface Resistance 2.00e+15 ohm
2.00e+15 ohm
ASTM D257
Dielectric Constant 4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
ASTM D150
4.9

@Frequency 1e+6 Hz
4.9

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Dissipation Factor 0.0080

@Frequency 1e+6 Hz
0.0080

@Frequency 1e+6 Hz
ASTM D150
0.0090

@Frequency 100 Hz
0.0090

@Frequency 100 Hz
ASTM D150
Arc Resistance >= 300 sec
>= 300 sec
UL 746A
Comparative Tracking Index 550 V
550 V
Hot Wire Ignition, HWI >= 150 sec
>= 150 sec
High Amp Arc Ignition, HAI 74 arcs

@Thickness 0.800 mm
74 arcs

@Thickness 0.0315 in
High Voltage Arc-Tracking Rate, HVTR 16.0 mm/min
0.630 in/min
Processing Properties Metric English Comments
Melt Temperature 321 - 343 °C
610 - 649 °F
Injection
Users viewing this material also viewed the following: