Mechanical Properties Metric English Comments
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer
Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con..
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and ExtrudedRoHS CompliantInformation provid..
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer
Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c..
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C..
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Tensile Strength at Break 1.03 MPa
150 psi
ASTM D412
Teknor Apex Uniprene® UN-1674C Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Tensile Strength at Break 1.03 MPa
150 psi
ASTM D638 - ISO 527-2
DuPont Keldax® 6705B Filled Thermoplastic Ethylene Polymer
A filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailability: Nor..
Tensile Strength at Break 1.03 - 1.38 MPa
150 - 200 psi
Abatron AboSeal 8104-9 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk
AboSeal 8104-9 is a 2-part, 100% solids, thixotropic or self-leveling polysulfide. It comes in most colors. It has been made to meet Federal Spec. TT-S-00227-E. It is preferred when white or light c..
Tensile Strength at Break 1.03 MPa
149 psi
ASTM D4325
3M Scotch™ 2228 Rubber Mastic Tape
3M™ Scotch™ 2228 is a conformable self-fusing rubber electrical insulating sealing tape. Scotch 2228 consist of an ethylene propylene rubber (EPR) backing coated with an aggressive, temperature-st..
Tensile Strength at Break 1.03 MPa
150 psi
ASTM D412