Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1100 MPa | 160000 psi | ASTM E345-93, Type A Specimen |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |
|||
Tensile Strength at Break | 1100 MPa | 160000 psi | Hard |
California Fine Wire Alloy 443 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 1100 MPa | 160000 psi | R<sub>m</sub>. 500°C tempering temperature. Quenching in oil ø 120. Testpiece hardened by oil quenching from 850°C. |
Assab Steels 705M Machinery Steel ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde.. |
|||
Tensile Strength at Break | 1100 - 1900 MPa | 160000 - 276000 psi | Longitudinal |
Goodfellow Carbon/Epoxy Composite Rod Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |