Mechanical Properties Metric English Comments
Tensile Strength at Break 1100 MPa
160000 psi
ASTM E345-93, Type A Specimen
NiCoForm NiColoy® E Electroformed Nickel-Cobalt
NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi..
Tensile Strength at Break 1100 MPa
160000 psi
Hard
California Fine Wire Alloy 443 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.
Tensile Strength at Break 1100 MPa
160000 psi
R<sub>m</sub>. 500°C tempering temperature. Quenching in oil ø 120. Testpiece hardened by oil quenching from 850°C.
Assab Steels 705M Machinery Steel
ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde..
Tensile Strength at Break 1100 - 1900 MPa
160000 - 276000 psi
Longitudinal
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.