Polymer Property : Tensile Strength at Break = 1900 MPa
Polymer Property :
Tensile Strength at Break =
1900 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
1100
-
1900
MPa
160000
-
276000
psi
Longitudinal
Goodfellow Carbon/Epoxy Composite Rod
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.