Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Strength at Break | 78.5 MPa @Temperature 23.0 °C |
11400 psi @Temperature 73.4 °F |
ISO 527-2/5 |
PolyOne Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Strength at Break | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 78.5 MPa | 11400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
Chase Plastics CP Pryme® NN113GL (COND, 50% RH) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 78.3 MPa | 11400 psi | ASTM D3759 |
3M 8992 Polyester Tape 3M™ Polyester Tape 8992 is a dark green polyester tape with silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag.. |
|||
Tensile Strength at Break | 78.3 MPa | 11400 psi | ASTM D3759 |
3M 8992L Polyester Tape 3M™ Polyester Tape 8992L is a dark green polyester tape with silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and ba.. |
|||
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
PlastxWorld CEVIAN® S5210 10% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |
|||
Tensile Strength at Break | 78.5 MPa | 11400 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
PlastxWorld CEVIAN®-N 080 SAN resin These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |