Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.6 MPa | 2260 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength at Break | 15.6 MPa | 2260 psi | ASTM D638 |
Teknor Apex APEX® 84137 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Cable Jacketing Agency Ratings: UL 62 Wire Types: SAE; SJTW; SPT-1; SPT-2; SPT-3; SRDT; STW; SVTForms: PelletsIn.. |
|||
Tensile Strength at Break | 15.6 MPa | 2260 psi | Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F) |
3M Dyneon™ PFE 132TBZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 132TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F.. |
|||
Tensile Strength at Break | 15.6 MPa | 2260 psi | Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F) |
3M Dyneon™ PFE 191TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 81TZ, PFE 131TZ and PFE 191TZ are technically advanced high temperature perfluorelastomers (HT PFE). They are designed to meet the challenges of higher temperature applications. Th.. |