Polymer Property : Tensile Strength at Break = 2260 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.6 MPa
2260 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Tensile Strength at Break 15.6 MPa
2260 psi
ASTM D638
Teknor Apex APEX® 84137 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Cable Jacketing Agency Ratings: UL 62 Wire Types: SAE; SJTW; SPT-1; SPT-2; SPT-3; SRDT; STW; SVTForms: PelletsIn..
Tensile Strength at Break 15.6 MPa
2260 psi
Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F)
3M Dyneon™ PFE 132TBZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 132TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F..
Tensile Strength at Break 15.6 MPa
2260 psi
Press Cure 15 Minutes @ 188°C (370°F), Post Cure 24 Hours @ 250°C (482°F)
3M Dyneon™ PFE 191TZ High Temperature Perfluoroelastomer
3M™ Dyneon™ PFE 81TZ, PFE 131TZ and PFE 191TZ are technically advanced high temperature perfluorelastomers (HT PFE). They are designed to meet the challenges of higher temperature applications. Th..