Material Notes:
Applications: ExtrusionRAPREX® R100D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched structure. It is a thermoplastic resin and is fully recyclable. Due to its broad molecular weight distribution and melt strength, RAPREX® R100D is used for pipes, extruded profiles, sheet and large blow molded articles. Raprex® R100D contains a robust stabilization package providing excellent melt stability as well as long-term heat aging.Information provided by Sterigenics
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D792
Melt Index of Compound 0.26 g/10 min

@Load 10.0 kg,
Temperature 190 °C
0.26 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.9 MPa
2450 psi
ASTM D638
Tensile Strength, Yield 28.6 MPa
4150 psi
ASTM D638
Elongation at Break 43 %
43 %
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 0.869 GPa
126 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
Partial Break; ASTM D256
0.700 J/cm

@Temperature -40.0 °C
1.31 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746