Mechanical Properties Metric English Comments
Tensile Strength at Break 12.9 MPa
1870 psi
ASTM D1414
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer
Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 p..
Tensile Strength at Break 12.9 MPa
1870 psi
ASTM D412
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 12.9 MPa
1870 psi
ASTM D412
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 12.9 MPa
1870 psi
Daikin DAI-EL G-575 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 70% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low permeability to gasoline and a..
Tensile Strength at Break 12.9 MPa
1870 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2261Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2261Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
Tensile Strength at Break 12.9 MPa
1870 psi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2211 Fluoroelastomer
Dyneon FC 2211 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The "dry" ingre..
Tensile Strength at Break 12.9 MPa
1870 psi
ASTM D412
Teknor Apex APEX® 2565-H Polyvinyl Chloride, Flexible