Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 215 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa
31200 psi
50 mm/min; ASTM D638
Ovation Polymers Opnyl OP6GF43 Nylon 6, 43% Glass Reinforced, Dry
Nylon 6 - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m..
Tensile Strength at Break 215 MPa
31200 psi
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Tensile Strength at Break 215 MPa
31200 psi
ISO 527-1, -2; 5 mm/min
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Tensile Strength at Break 215 MPa
31200 psi
ISO 527 Type 1A
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY
Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati..
Tensile Strength at Break 215 MPa
31200 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66
LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive.
Tensile Strength at Break 215 MPa
31200 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI
LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
Tensile Strength at Break 215 MPa
31200 psi
ISO 527-1/-2
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned
Information provided by Unitika Ltd.
Tensile Strength at Break 215 MPa
31200 psi
ISO 527-93
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Tensile Strength at Break 215 MPa
31200 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30
Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca..
Tensile Strength at Break 215 MPa
31200 psi
5 mm/min; ISO 527
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Strength at Break 215 MPa
31200 psi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50
Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:..
Tensile Strength at Break 215 MPa
31200 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 215 MPa
31200 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide with Improved Surface Appearance Zytel HTN51G35HSLR BK420J is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin w..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also..
Tensile Strength at Break 215 MPa
31200 psi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Tensile Strength at Break 215 MPa
31200 psi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Tensile Strength at Break 215 MPa
31200 psi
ISO 527
Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Strength at Break 215 MPa
31200 psi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-50 PA6-GF50
Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su..
Tensile Strength at Break 215 MPa
31200 psi
5 [mm/min]; ISO 527-1/2
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Tensile Strength at Break 215 MPa

@Temperature -40.0 °C
31200 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and ..
Tensile Strength at Break 215 MPa

@Temperature -40.0 °C
31200 psi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and ..
Tensile Strength at Break 215 MPa
31200 psi
5 [mm/min]; ISO 527-1/2
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Tensile Strength at Break 215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G35HSLR BK420J is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearance. It is also a PPA resin..
Copyright © lookpolymers.com All Rights Reserved