Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK
LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber.
Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10
LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber.
Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF007 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Tensile Strength at Break 176 MPa
25500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66
LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive.
Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
Chase Plastics CP Pryme® N130GL (DAM) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
Chase Plastics CP Pryme® N130L Nylon 6, 30% Glass Fiber Reinforced, Lubricated
Features: LubricatedForm: PelletsInformation provided by Chase Plastics.