Chase Plastics CP Pryme® N130GL (DAM) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N130GL (DAM) Nylon 6, 30% Glass Fiber Reinforced, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 176 MPa
25500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 269 MPa
39000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648