Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Metal Filled
Manufacturer Abatron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 15 lbs/gal; B: 9.8 lbs/gal; mixing ratios: A/B: 100/8.3 pbw (100/12.6 pbv); pot life: 5-8 hours; bronze color; Requires heat cure: 1-12 hours at 176-302° F (80-150° C). The Mastershop compounds are versatile, high-impact and wear resistant, and permanent. Good adhesion to metals, ceramics, glass, wood, fiberglass, masonry, and most rigid materials. Dimensionally stable and shrink-free. Almost unlimited shelf-life. Unaffected by atmospheric conditions, salt and fresh water, alkalis, diluted acids, many solvents, oils, and greases. Withstand temperatures up to 100° C (212° F) or 160° C for the “H” versions. Cured material is easy to machine with standard tools. Can be applied in any thickness. Ample working time.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0424 lb/in³
Part B
1.80 g/cc
0.0649 lb/in³
Part A
Mechanical Properties Metric English Comments
Hardness, Shore D 83 - 87
83 - 87
Tensile Strength at Break 3.45 - 41.4 MPa
500 - 6000 psi
Flexural Strength 3.45 - 48.3 MPa
500 - 7000 psi
Compressive Strength 62.1 - 89.6 MPa
9000 - 13000 psi
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Processing Properties Metric English Comments
Cure Time 60.0 - 720 min

@Temperature 80.0 - 150 °C
1.00 - 12.0 hour

@Temperature 176 - 302 °F
Pot Life 300 - 480 min
300 - 480 min
Descriptive Properties Value Comments
Color Bronze
Parts by Weight (pbw) 100
Part A
8.3
Part B