Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-447 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9902 Very Dark Gray Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | ASTM D638 |
LyondellBasell Petrothene® LM600500 High Density Polyethylene ApplicationsPETROTHENE LM 6005-00 resin is especially designed for water, milk, and juice bottles. It exhibits excellent rigidity and good processability.Regulatory StatusLM 6005-00 meets the requi.. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min.; ASTM D638 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | 2 in/min; ASTM D638 |
Ineos TUB 121NTW HDPE TUB121 NTW is a natural high density bimodal polyethylene copolymer designed for extrusion of large diameter, thick wall piping for potable water, industrial and mining applications. When blended wi.. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | |
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | ASTM D638 |
Chase Plastics CP Pryme® PE-200-HD8M General Purpose High Density Polyethylene Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D638 |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | vs. steel; 3 s set time |
Elmer's Products Aron Alpha® 801 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.Low gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. .. |
|||
Tensile Strength at Break | 30.3 MPa | 4400 psi | vs. steel; 15 s set time |
Elmer's Products Aron Alpha® 802 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.Medium gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrate.. |
|||
Tensile Strength at Break | 30.3 MPa | 4390 psi | ASTM D3756 |
3M 201+ General Use Masking Tape 3M™ General Use Masking Tape 201+ is a tan colored crepe paper masking tape for holding, bundling, sealing, non-critical masking applications and a vast number of other jobs where a pressure sensit.. |