Mechanical Properties Metric English Comments
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Eastman Tenite 360A4861316 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp
Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D3756
3M 201+ General Use Masking Tape
3M™ General Use Masking Tape 201+ is a tan colored crepe paper masking tape for holding, bundling, sealing, non-critical masking applications and a vast number of other jobs where a pressure sensit..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D3756
3M 200 Paper Tape
3M™ Paper Tape 200 is a utility purpose paper tape for holding, bundling, sealing, non-critical masking and a vast number of other jobs where a pressure-sensitive tape is needed.Information provide..
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..