Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 310 - 379 MPa | 45000 - 55000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in.. |
|||
Tensile Strength at Break | 310 - 379 MPa | 45000 - 55000 psi | 1020 Steel butt joint |
Lucas-Milhaupt BRAZE 716 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp.. |
|||
Tensile Strength at Break | 310 - 379 MPa | 45000 - 55000 psi | 1020 Steel butt joint |
Lucas-Milhaupt BRAZE 716 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp.. |
|||
Tensile Strength at Break | 331 - 379 MPa | 48000 - 55000 psi | Strip, Temper-Ex. Spring |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |
|||
Tensile Strength at Break | 331 - 379 MPa | 48000 - 55000 psi | Wire, Temper-Ex. Spring |
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and .. |