Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 55000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 310 - 379 MPa
45000 - 55000 psi
Nickel-Silver butt joint
Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in..
Tensile Strength at Break 310 - 379 MPa
45000 - 55000 psi
1020 Steel butt joint
Lucas-Milhaupt BRAZE 716 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp..
Tensile Strength at Break 310 - 379 MPa
45000 - 55000 psi
1020 Steel butt joint
Lucas-Milhaupt BRAZE 716 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp..
Tensile Strength at Break 331 - 379 MPa
48000 - 55000 psi
Strip, Temper-Ex. Spring
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and ..
Tensile Strength at Break 331 - 379 MPa
48000 - 55000 psi
Wire, Temper-Ex. Spring
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Commercial grade fine silver (99.90% minimum silver) is widely used in numerous electrical, electronic, and industrial applications, such as contacts, fuse elements, lead wires, battery plated, and ..