Material Notes:
3M Scotchcast Electrical Insulating Resin 4 is a two-part, epoxy insulating and encapsulating resin. This resin, mixed in its unique two-part bag, generates its own heat to cure. Its compatibility with solid and synthetic cable insulations and jackets makes Resin 4 an excellent insulator and sealer for cable splicing. Use Resin 4 to splice solid dielectric and oil-filled cables up to 8 kV and to jacket high voltage power cables. It is used in 3M Splice Kit Series 82 and 90-B1.Information provided by 3M
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Moisture Absorption 2.60 %
2.60 %
7 days at RT
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength at Break 33.8 MPa
4900 psi
ASTM D412
Elongation at Break 4.0 %
4.0 %
ASTM D412
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 54.0 °C
129 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.1

@Frequency 60.0 Hz,
Temperature 23.0 °C
3.1

@Frequency 60.0 Hz,
Temperature 73.4 °F
ASTM D150
3.9

@Frequency 60.0 Hz,
Temperature 60.0 °C
3.9

@Frequency 60.0 Hz,
Temperature 140 °F
ASTM D150
6.0

@Frequency 60.0 Hz,
Temperature 90.0 °C
6.0

@Frequency 60.0 Hz,
Temperature 194 °F
ASTM D150
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Dissipation Factor 0.50

@Frequency 60.0 Hz,
Temperature 23.0 °C
0.50

@Frequency 60.0 Hz,
Temperature 73.4 °F
ASTM D150
Processing Properties Metric English Comments
Gel Time 16.0 min
16.0 min
ASTM D2471-99
Descriptive Properties Value Comments
Appearance Black