Polymer Property : Tensile Strength at Break = 4930 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.0 - 34.0 MPa
4640 - 4930 psi
ASTM D4745-97
Adamas Adalon® 509 PTFE, 3% MoS2
Information provided by Adamas, HPM
Tensile Strength at Break 17.0 - 34.0 MPa
2470 - 4930 psi
ASTM D638
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Tensile Strength at Break 17.0 - 34.0 MPa
2470 - 4930 psi
ASTM D638
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Tensile Strength at Break 17.0 - 34.0 MPa
2470 - 4930 psi
ASTM D638
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Tensile Strength at Break 32.0 - 34.0 MPa
4640 - 4930 psi
ASTM D4745-97
Adamas Adalon® 508 PTFE, 1% MoS2
Information provided by Adamas, HPM
Tensile Strength at Break 32.0 - 34.0 MPa
4640 - 4930 psi
ASTM D4745-97
Adamas Adalon® 510 PTFE, 5% MoS2
Information provided by Adamas, HPM
Tensile Strength at Break 17.0 - 34.0 MPa
2470 - 4930 psi
ASTM D638
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..