Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.43 MPa @Temperature 23.0 °C |
788 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Tensile Strength at Break | 5.43 MPa @Temperature 23.0 °C |
788 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |