Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 788 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.43 MPa

@Temperature 23.0 °C
788 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Tensile Strength at Break 5.43 MPa

@Temperature 23.0 °C
788 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp..