Mechanical Properties Metric English Comments
Tensile Strength at Break 39.3 MPa
5700 psi
2 in/min; ASTM D638
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade
Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade
General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B9025 , 8% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength at Break 39.3 MPa
5700 psi
Injection molded parts; ISO 37
Huntsman IROGRAN® A 80 H 4826 TPU-Polyester
Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and hig..
Tensile Strength at Break 39.3 MPa
5700 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded
Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc.
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D 638
Shakespeare Isocorâ„¢ SVP4011 high viscosity PA-6/69
Isocorâ„¢ 4011 is a high viscosity PA-6/69. This resin is specifically suited for applications requiring superior toughness and abrasion resistance. Isocorâ„¢ 4011 is also used in applicat..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Chase Plastics CP Pryme® N300HSL (COND, 50% RH) Nylon 6 (Utility Grade), Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Chase Plastics CP Pryme® N300L (COND, 50% RH) Nylon 6 (Utility Grade), Internally Lubricant
Information provided by Chase Plastics.
Tensile Strength at Break >= 39.3 MPa
>= 5700 psi
ASTM D 638 type IV
Total 54050 HDPE, blow molding
Applications: 55-gallon shipping containers, open-top drums, industrial tanks, agricultural chemical tanks. Blow Molding Stock Temperature 380 – 450 ºF Extrusion melt temperature 400 - 480ºFInfor..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D3759
3M 433L Premium Performance Aluminum Foil Tape
Linered version of 433Information provided by 3M
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Aaron Industries AAROLENE® ARPS 100-1 GPPS BLACK Polystyrene Compounded Resin
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A reprocessed, general-purpose Polystyrene resin, compounded black, specifically designed for all high speed injection molding appli..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 8% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..