Material Notes:
Applications: 55-gallon shipping containers, open-top drums, industrial tanks, agricultural chemical tanks. Blow Molding Stock Temperature 380 – 450 ºF Extrusion melt temperature 400 - 480ºFInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 200 hour
>= 200 hour
ASTM D1693 cond. B 10% lgepal
>= 1000 hour
>= 1000 hour
ASTM D1693 cond. B 100% lgepal
High Load Melt Index 5.5 g/10 min

@Load 21.6 kg
5.5 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 39.3 MPa
>= 5700 psi
ASTM D 638 type IV
Tensile Strength, Yield >= 28.3 MPa
>= 4100 psi
ASTM D 638 type IV
Elongation at Break >= 600 %
>= 600 %
ASTM D 638, type IV
Flexural Modulus 1.31 GPa
190 ksi
ASTM D 790
Izod Impact, Notched 6.67 J/cm

@Thickness 3.17 mm
12.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 128 °C
263 °F
ASTM D3417