3M 433L Premium Performance Aluminum Foil Tape

Category Metal , Nonferrous Metal , Aluminum Alloy , Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 433L Premium Performance Aluminum Foil Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linered version of 433Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Backing; ASTM D3652
88.9 microns
3.50 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D3759
Peel Strength 0.4163 kN/m
2.375 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 316 °C
601 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Descriptive Properties Value Comments
Adhesive Type Silicone