Polymer Property : Tensile Strength at Break = 580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.00 - 4.00 MPa
290 - 580 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9110/9410/9210/9310 Rubber-like Prototyping Polymer
Primary material: TangoBlackSecondary material: VeroWhitePlus, VeroBlue, VeroBlack, FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific concen..
Tensile Strength at Break 2.00 - 4.00 MPa
290 - 580 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9860/9760 Rubber-like Prototyping Polymer
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu..
Tensile Strength at Break 2.00 - 4.00 MPa
290 - 580 psi
ASTM D412
Proto3000 Objet Digital Materials™ DM_9870/9770 Rubber-like Prototyping Polymer
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu..
Tensile Strength at Break 3.00 - 4.00 MPa
435 - 580 psi
ASTM D4745-97
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber
Information provided by Adamas, HPM