Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D412 |
Multibase TPSiV™ 3340-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D412 |
Multibase TPSiV™ 3340-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 37 |
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 37 |
PolyOne OnFlex™ S KA 40A-3S1767 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 37 |
PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Tensile Strength at Break | 3.00 - 5.00 MPa | 435 - 725 psi | ASTM D412 |
Proto3000 Objet Digital Materials™ DM_9120/9420/9220/9320 Rubber-like Prototyping Polymer Primary material: TangoBlackSecondary material: VeroWhitePlus, VeroBlue, VeroBlack, FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific concen.. |
|||
Tensile Strength at Break | 3.00 - 5.00 MPa | 435 - 725 psi | ASTM D415 |
Proto3000 Objet TangoGray FullCure950 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | After Curing |
Silikony Polskie Gumosil T Silicone Rubber Hard, resistant to sudden and extensive temperature changes |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 37 |
ELASTO UK Dryflex® 3005-101 TPE, Modified Injection Molding Grade for Vacuum Cleaner Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3005-101 is specifically designe.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 400601S SBS Based Material, 60A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 37 |
ELASTO UK Dryflex® 5014-101 TPE, Modified Injection Molding Grade for General Applications The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5014-101 is specifically designe.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 502300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 602300S SEBS Based Material, Filled Qualities, 30A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 602350S SEBS Based Material, Filled Qualities, 35A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 662300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
ELASTO UK Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ASTM D638 |
Arkema Group LOTRYL® 28 BA 175 Copolymer Ethylene - Butyl Acrylate LOTRYL® 28 BA 175 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 28% in weight. LOTRYL® 28 BA 175 is particularly.. |
|||
Tensile Strength at Break | 3.00 - 4.00 MPa | 435 - 580 psi | ASTM D4745-97 |
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber Information provided by Adamas, HPM |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, Conditioned Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Tensile Strength at Break | 3.00 MPa | 435 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX E 35.1 TPE-V, Shore A35 TPE-VInformation provided by BARLOG plastics GmbH. |