Polymer Property : Tensile Strength at Break = 68.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.0 - 68.0 MPa
9140 - 9860 psi
ASTM D638
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer
Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo..
Tensile Strength at Break 66.0 - 68.0 MPa
9570 - 9860 psi
ASTM D638
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi..
Tensile Strength at Break 58.0 - 68.0 MPa
8410 - 9860 psi
ASTM D638
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer
Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView ..