Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.50 MPa | 1090 psi | ISO 37 |
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Strength at Break | 7.50 MPa | 1090 psi | ASTM D412 |