Polymer Property : Tensile Strength at Break = 1090 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.50 MPa
1090 psi
ISO 37
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE)
OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Strength at Break 7.52 MPa
1090 psi
Across flow; ASTM D412
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Strength at Break 7.52 MPa
1090 psi
0.025" extruded film; ASTM D412
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN ..
Tensile Strength at Break 7.50 MPa
1090 psi
ASTM D412
Sumitomo Chemical ESPOLEX® 3885 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Tensile Strength at Break 7.52 MPa
1090 psi
ASTM D412
Teknor Apex Telcar® OBC 4873A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 7.52 MPa
1090 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Tensile Strength at Break 7.52 MPa
1090 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 191-85PA Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft ..