Material Notes:
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-density grades that can provide substantial weight and cost savings over higher-density thermoplastic elastomers. In this regard, SUMITOMO CHEMICAL introduces specific gravity as a significant factor in reducing unit cost and weight. Products molded from ESPOLEX® TPE Series exhibit rubber-like properties that range from a soft elastic to a semi-hard rubber material. Like all thermoplastic elastomers, ESPOLEX® TPE Series offers substantial savings over thermoset rubber in manufacturing since it is processed using standard thermoplastic processing equipment and techniques, and it does not require the vulcanization required by conventional rubbers.Information provided by Sumitomo Chemical
Physical Properties Metric English Comments
Density 0.880 g/cc
0.0318 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min

@Load 2.20 kg
1.5 g/10 min

@Load 4.86 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
10 Sec Delay; ASTM D2240
85
85
0 Sec Delay; ASTM D2240
Tensile Strength at Break 7.50 MPa
1090 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Flexural Modulus 0.0550 GPa
7.98 ksi
ASTM D790
Compression Set 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ASTM D395
55 %

@Temperature 70.0 °C
55 %

@Temperature 158 °F
ASTM D395
Processing Properties Metric English Comments
Middle Barrel Temperature 200 - 240 °C
392 - 464 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F