Mechanical Properties Metric English Comments
Tensile Strength at Break 650 MPa
94300 psi
6 lb. load and 0.009 in. diameter
Shakespeare WonderThread® SN-38 High tenacity TEX# 45 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..
Tensile Strength at Break 650 - 880 MPa
94300 - 128000 psi
Schmolz + Bickenbach UGICHROM 4362 Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 650 - 880 MPa
94300 - 128000 psi
Schmolz + Bickenbach UGICHROM 4462 Duplex Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength at Break 650 MPa
94300 psi
Goodfellow Chromaloy O® Resistance Alloy
Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information ..
Tensile Strength at Break 650 - 1100 MPa
94300 - 160000 psi
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Information provided by Goodfellow.
Tensile Strength at Break 650 - 820 MPa
94300 - 119000 psi
ThyssenKrupp PAS 600 Structural Steel for Cold Forming
This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio..
Tensile Strength at Break 650 - 1000 MPa
94300 - 145000 psi
Goodfellow Aluchrom O® Resistance Alloy
Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information ..