Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ISO 868 |
ExxonMobil Santoprene® 241-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 8221-65M300 Thermoplastic Vulcanizate - UV Resistant A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 8191-60B500 Thermoplastic Vulcanizate
(discontinued **) Product Description: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, PA 12.. |
|||
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 8291-60B500 Thermoplastic Vulcanizate
(discontinued **) Product Description: A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, P.. |