Mechanical Properties Metric English Comments
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for ..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ISO 868
ExxonMobil Santoprene® 241-55 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate
Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 8221-65M300 Thermoplastic Vulcanizate - UV Resistant
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 8191-60B500 Thermoplastic Vulcanizate  (discontinued **)
Product Description: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, PA 12..
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 8291-60B500 Thermoplastic Vulcanizate  (discontinued **)
Product Description: A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, P..