Mechanical Properties Metric English Comments
Tensile Stress 140 MPa

@Thickness 0.0500 mm
20300 psi

@Thickness 0.00197 in
ASTM D882-02
NeXolve LaRC™-CP1 Conductive Black Polyimide
Lower RF loss than other black and conductive black polyimides. NeXolve’s Conductive Black LaRC™-CP1 Polyimide is filled with carbon nanoparticles to produce a conductive black polyimide material ..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.dynamic stressReduced moment of inertia compared with metal parts.Be..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Tensile Stress 140 MPa
20300 psi
ISO 527-2
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
Tensile Stress 140 MPa
20300 psi
ISO 527-2
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
Tensile Stress 140 MPa
20300 psi
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Copyright © lookpolymers.com All Rights Reserved